Features of aluminium strip for tearing aluminium cap
The aluminium strip for tearing aluminium cap should be clean inside and outside light, no residual lubricant, burrs and damage, basically the same color, the tensile strength shall not be less than - 130mm², elongation of not less than 3%.
Tearing Aluminium Cap Strip Coating firmness:
the outer surface of the coating is121℃+/-2℃for 30 minutes, including 130℃+/-2℃for 5 minutes after steam sterilization, soaked with 80% alcohol cotton to wipe the surface for 30 seconds, and then soaked with 70% isopropyl alcohol cotton to wipe the surface for 30 seconds, the surface should be no wear.
Tearing Aluminium Cap Strip Breaking tension:
The maximum tearing force of the tearing aluminium cap is 5--15N, and the fracture is not allowed during the tearing process.